Introducing Atom Arc 7018 Acclaim. The newest addition to the Atom Arc line of stick electrodes, Atom Arc Acclaim offers the same drive and dig of ESAB’s popular Atom Arc stick electrode with improved weld puddle control resulting in easier out-of-position welding.
Atom Arc 7018 Acclaim provides the deep, penetrating arc and tough mechanical properties of the original Atom Arc 7018 with excellent control in out-of-position welding applications, greater weld puddle control and easier arc initiation. The new electrode also features excellent ease of use for both novice and experienced welders, a wide operating range and minimal clean up. It meets E7018H4R classification.